GregorTacTac@lemm.ee to 3DPrinting@lemmy.worldEnglish · 8 months agoShit posting but 3d this timefiles.catbox.moeimagemessage-square33fedilinkarrow-up172file-text
arrow-up172imageShit posting but 3d this timefiles.catbox.moeGregorTacTac@lemm.ee to 3DPrinting@lemmy.worldEnglish · 8 months agomessage-square33fedilinkfile-text
minus-squareDumnorix@lemmy.worldlinkfedilinkEnglisharrow-up3·edit-28 months agoHere’s a scientific paper about it. :) https://medialibrary.uantwerpen.be/oldcontent/container11343/files/bonding_pla_with_salt_water_v20160713.pdf A brine is a much cleaner solution than the usual advices of hairspray or tape. Just be careful not to put salt on your electronics.
Here’s a scientific paper about it. :) https://medialibrary.uantwerpen.be/oldcontent/container11343/files/bonding_pla_with_salt_water_v20160713.pdf
A brine is a much cleaner solution than the usual advices of hairspray or tape. Just be careful not to put salt on your electronics.
Thanks!